Welding & Preservation » Underwater Welding Overview
Special 25 CrMo 4 steel - Underwater welding using temper-bead technology in water 36 metres deep - Well depth: 70 metres read more »
Improved technologies and enhanced qualification and training have made it possible to provide high-quality performance in underwater welding today. read more »
The sheet piling around berths 7, 9 and 11 had become so rusty and weak in places that urgent repair and rehabilitation work was required. read more »
Sheet steel piling walls erected in bodies of water are especially prone to corrosion in the splash zone, i.e. in the transition area from air to water, and particularly in salty tidal water. This area usually comprises +1 metre to -2 metres above or below sea level. read more »